Materials
|
Working Temp. Max.( ℃)
|
Working Environment
|
Stainless steel
|
380
|
Nitric acid, Sulphuric acid, Acetic acid, Oxalic acid, Phosphoric acid, 5 %hydrochloric acid, Fused sodium,Liquid hydrogen, Liquid nitrogen, Sulfureted hydrogen, Acetylene, Water vapour, Hydrogen, Coal gas, Carbon dioxide gas
|
Titanium
|
280 (wet)
|
Nitric acid, Fluoride salts, Lactic acid, Wet chlorine, Seawater, Atmosphere and etc.
|
Bronze
|
300
|
Organic solvent, Fuel, Atmosphere, Neutral water and oil
|
Monel
|
500
|
Chloride,Chloride gas and liquid.
|
Hastelloy
|
930
|
Normal or high temperature hydrochloric acid, organicacid, non-oxidated acid, non-oxidatedsalt liquid, oxidated acid, Oxidated Salts, Seawater.
|
Inconel
|
800
|
Suitable for most of the organic acid and organic compound
|
UHMW-PE
|
80
|
Acid, Alkali, organic solvent, etc.
|
PTFE
|
200
|
Acid, Alkali, organic solvent, high temperature, etc.
|